Current-induced DW velocity in ultrathin freestanding heterostructures (25 A Pt, no MgO buffer). Cyan, black, and red curves correspond to measurements taken immediately after fabrication, after 1.5 years of air exposure, and after 2 h of annealing in air at 100 °C, respectively.