CpGFP-K72-atto390 (10 mol%) glue responded to both cohesive and adhesive failure. The data obtained from the PS samples (f,g) after lap shear testing was inhomogeneous and included unaltered zones (green) and damaged zones (blue). Mean values ± SD from the mean. N= 3 different lap shear tests. P-values calculated using Student's t-test (two-sided), *P< 0.05, **P< 0.01, ***P< 0.001.