Change in stress state in the LB front region, showing three stress components at a tensile strain of 4%. The top and bottom panels show σ yy , σ xx and σ zz along the length, width and thickness directions of the tensile sample, respectively. The arrow indicates the LB propagation direction towards the deformation-free gauge section.