Scatter Plot from Scientific Research

CC-BY
2
Views
0
Likes
Citation
Durability test of the photothermal-pneumatic actuation under 5000 stepwise deformation-recovery cycles. The inset shows the maximum deformation height achieved during 50 continuous actuation cycles.
#Scatter Plot#Durability Test#Photothermal-Pneumatic Actuation#Stepwise Deformation-Recovery Cycles#Deformation Height#Actuation Cycles